Pressure Drop
Polymer melt flows from high pressure areas to low pressure areas. The results of this
analysis display the pressure drop through the cavity. The pressure drop test uses a
range of color to indicate the region of lowest pressure(colored blue) through the region
of the highest pressure drop (colored red). Ideally, the pressure drop should be uniform
from the plastic injection location to the last point of to fill.

|